![](http://tiebapic.baidu.com/forum/w%3D580/sign=0828f186c035e5dd902ca5d746c4a7f5/a51c758da9773912f4f194b5bd198618377ae22a.jpg?tbpicau=2025-02-25-05_39c6d911bf41ffee3bbd020576719b8e)
![](http://tiebapic.baidu.com/forum/w%3D580/sign=206d98fec318367aad897fd51e728b68/c3f070c6a7efce1b0d2a9d1dea51f3deb58f6587.jpg?tbpicau=2025-02-25-05_709fb3d288214546187e2b11a1676a4f)
![](http://tiebapic.baidu.com/forum/w%3D580/sign=a026906bc95494ee87220f111df7e0e1/d8cbb51c8701a18bd42e039bdb2f07082938fe38.jpg?tbpicau=2025-02-25-05_da155668243833763d402eca7ce9178c)
![](http://tiebapic.baidu.com/forum/w%3D580/sign=539b69366a2eb938ec6d7afae56385fe/9ce318178a82b9014deca9e4368da9773812ef47.jpg?tbpicau=2025-02-25-05_e926c71bfc0ca4bba5cf6b60eaea4abc)
![](http://tiebapic.baidu.com/forum/w%3D580/sign=a7454865c50a19d8cb03840d03f882c9/faf38c13632762d09cf9b56be5ec08fa503dc63a.jpg?tbpicau=2025-02-25-05_e6251d0f5cbf30c9ca514c2d0bfe3eb8)
![](http://tiebapic.baidu.com/forum/w%3D580/sign=b512f9f9edd3fd1f3609a232004f25ce/5be5573d269759ee0af40a1cf7fb43166c22df64.jpg?tbpicau=2025-02-25-05_51ade015f8772e1c6ecb9097ad46e813)
![](http://tiebapic.baidu.com/forum/w%3D580/sign=d06aa6bb553853438ccf8729a312b01f/f807912bd40735fa038d1b6edb510fb30e240883.jpg?tbpicau=2025-02-25-05_9d35ce49cb578e3ae18570bac1a30855)
本材料适用于纯棉和含棉量达到或者超过30%的面料进行热升华印染及数码印花,实现了棉类天然纤维热升华印染和数码印花的工艺和技术改革。
干擦湿擦色牢度4.5级以上、抗紫外线照射测试时间超过400小时以上、色彩还原新鲜。工艺过程中不需使用一滴水和一立方MM3水蒸汽,彻底解决了纯棉印染大量废水排放和高能耗的难题。
①、固色桨涂层为水剂型状态
本产品呈水剂型状态,符合各项环保标准。特别适用于纯棉帆布布匹的涂布和上浆,以及上浆后的热升华印花印染处理及加工。目前针织面料只能局部印染。
②、黑色不会变成红色
处理本涂层的纯棉帆布布匹,热升华烫画转印后,经过严苛的400小时紫外线照射测试,黑色色块不会变成红色。
③、参考烫画温度和时间
裁片烫画参数选择:210度/20秒,230度/8秒(平板烫画机得出的参考数据);
布匹烫画参数选择:与涤纶热升华滚筒烫画机的参数一样。
④、可以加增稠剂吗?
布料热升华印染后达不到您想要的好效果,或者是想要更好的效果。可以添加少量或适量的PTF增稠剂,提升粘度。达到更好的效果。因为固色桨涂层是水剂状的,如果面料吸水,就会把涂层吸入布料,影响效果。
⑤、适合哪些布料印染?
纯棉或者含棉量达到或者超过30%以上的帆布面料和针织面料。
注意:由于还存在一点手感,只适合纯棉帆布匹布上浆,针织纯棉只适合裁片及局部印花染色。